Barium titanate (BaTiO3)
Barium titanate (BaTiO3) single crystal has excellent photorefractive properties, high self-pumped phase conjugate reflectivity and two-wave mixing (optical amplification) efficiency, and has huge potential application prospects in optical information storage; At the same time it is also an important substrate substrate material.
Main performance parameters
|
||||||
Crystal structure
|
Tetragona(4m): 13°C <T <132°C a=3.99 ,c=4.04,(at 26°C)
|
|||||
density
|
6.02 (g/cm 3 )
|
|||||
Melting point
|
1612°C
|
|||||
Growth method
|
TSSG (Top Seeded Solution Growth)
|
|||||
Dielectric constant
|
ea=3700 ec=135 (free state)
|
|||||
ea=2400 ec=60 (blessed state)
|
||||||
Refractive index
|
|
515nm
|
633nm
|
800nm
|
||
n o
|
2.4912
|
2.4160
|
2.3681
|
|||
n o
|
2.4247
|
2.3630
|
2.3235
|
|||
Transmission wavelength range
|
0.43-6.30mm
|
|||||
Photoelectric coefficient
|
r1 T 3=8±2pm/V rT33=105±10pm/V rT42=1300±100pm/V
|
|||||
Self-pumped phase conjugate reflectivity
(0 degree cut)
|
50-70% for l = 515nm(Ce: BaTiO 3 )
|
|||||
40-60% (PureBaTiO 3 ) for l = 515nm
|
||||||
50-80% for l = 633nm(Ce: BaTiO 3 )
|
||||||
40-60% for l = 633nm (PureBaTiO 3 )
|
||||||
Two-wave mixing coupling coefficient
|
10 -40 cm -1
|
|||||
Absorption loss
|
l: 515nm
|
633nm
|
800nm
|
|||
a: 0.285cm -1
|
0.108cm -1
|
0.033cm -1
|
||||
Crystal orientation
|
<100>, <001>, <110>, <111>±0.5º
|
|||||
Size (mm)
|
10×10×1/0.5mm, 10×5×1/0.5mm, 5×5×1/0.5mm
Can be customized according to customer needs, special direction and size of the substrate
|
|||||
polishing
|
Single-sided or double-sided
|
|||||
Surface roughness
|
Surface roughness(Ra):<=10 A
Atomic particle microscope (AFM) test report is available |
|||||
Package
|
Class 100 clean bag, Class 1000 super clean room
|
|||||